One of Hottest for Reinforced Flexible Graphite Gasket for Mexico Importers
One of Hottest for Reinforced Flexible Graphite Gasket for Mexico Importers Detail:
The reinforced flexible graphite composite gasket is composed of pressed metal sheet and flexible graphite grain after pressing and cutting.
1.Characteristic
Reinforced graphite gasket has perfect corrosion resistance, high &low temperature resistance, excellent elastic resilience, good strength. It can be cut into complex shape. Reinforced graphite gasket with inner &outer coating keeps all the excellent characteristics of itself, besides, it could be easily installed, disassembled, undamaged, meanwhile can prevent from medium corrosion, improve the pressure resistance.
2.Technical Data Sheet
Reinforced Material |
Pressure Resistance |
Temperature |
Elongation(%) |
Recovery(%) |
|
Oxidizing Environment |
Non-Oxidizing |
||||
CS Reinforce Sheet |
≥48 |
-10-450 |
-10-550 |
30-35 |
15-20 |
SS304,SS316 Reinforced Sheet |
≥48 |
-240-450 |
-200-600 |
30-35 |
15-30 |
SS304,SS316 Sheet |
≥48 |
-240-450 |
-200-600 |
30-40 |
10-15 |
Ss304, Mesh Sheet |
≥48 |
-240-450 |
-200-600 |
40-50 |
15-20 |
Reinforced Material |
Breathable (cm3/min) |
Leakage |
Seal Constant |
||
N2 m1/hr |
Bumming oil A |
“M” |
“Y” |
||
CS Reinforce Sheet |
<=0.8 |
30 |
<0.5 |
3.0 |
9000 |
SS304,SS316 Reinforced Sheet |
<=0.8 |
60 |
<0.5 |
2.5 |
4000 |
SS304,SS316 Sheet |
<=0.4 |
35 |
<0.5 |
2.0 |
900 |
SS304, Mesh Sheet |
≥1.0 |
70 |
<0.5 |
3.0 |
5000 |
Product detail pictures:
Related Product Guide:
Comparison of O-Ring Materials
What Is A PTFE Ring Gasket?
One of Hottest for Reinforced Flexible Graphite Gasket for Mexico Importers, The product will supply to all over the world, such as: , , ,
Uno de los principales motivos de averia de las bombas benjamin radica en la suciedad interna y el mal funcionamiento del oring p30. En este video se muestra el paso a paso para realizar el mantenimiento, limpieza y cambio del oring en cuestion. Un video realizado por Field Target Colombia.
One of the main reasons of damage of the benjamin hand pump is related to the o-ring P-30. In this video we clean the internal parts and change the main o-ring. The video is in spanish but I hope it could help to anyone.
By from -
By from -